Reaction equation

Participants

RoleNameHCIDCharge
ReactantEthylene carbonateHCID 7303—
CatalystSodium StannateHCID 21977542—
ProductCarbon DioxideHCID 28019.2%
ProductEthylene carbonateHCID 730397.9%

Reaction Conditions

Temperature175 °C

Reaction Steps

A 10:1 mole ratio of ethylene carbonate to polyester polyol (poly(caprolactone) diol, MW=530) is heated with stirring under a nitrogen atmosphere for 4 hours at 175° C. using 0.5 percent sodium stannate trihydrate as catalyst to give 97.9 percent ethylene carbonate conversion to a poly(alkylene carbonate) polyol with 19.2 percent carbon dioxide. The catalyst is removed as in Example 1.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04709069
Source datasetuspto-grants-1987_11
ORD IDord-83e27cce764c40d789da328866ec9e7a
Source noteuspto-grants-1987_11