Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Ethylene carbonate | HCID 7303 | — |
| Catalyst | Potassium Carbonate | HCID 11430 | — |
| Solvent | Diethylene Glycol | HCID 8117 | — |
| Product | Carbon Dioxide | HCID 280 | 11.6% |
| Product | Ethylene carbonate | HCID 7303 | 95% |
Reaction Steps
A 10:1 mole ratio of ethylene carbonate to diethylene glycol is heated with stirring under a nitrogen atmosphere for 3 hours at 150° C. using 1.0 percent potassium carbonate as catalyst to give 95 percent ethylene carbonate conversion to a poly(alkylene carbonate) polyol with 11.6 percent carbon dioxide. The catalyst is removed as in Example 1.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US04709069 |
|---|
| Source dataset | uspto-grants-1987_11 |
|---|
| ORD ID | ord-5d1d4453fa034fca8947cb92bd7d41c0 |
|---|
| Source note | uspto-grants-1987_11 |
|---|