Acetaldehyde → Formaldehyde urea silicate

https://huagongshe.com/reaction/258524

Reaction equation

Participants

RoleNameHCIDCharge
ReactantAcetaldehydeHCID 177—
ReactantUrea silicateHCID 86734903—
ProductFormaldehyde urea silicateHCID 86734902—

Reaction Steps

One mol by weight of metasilicic acid and one mol by weight of urea are mixed, heated to 95° to 150° C. for 20 to 60 minutes, until the reaction is substantially complete, thereby producing white granules of urea silicate. The said urea silicate is mixed into about one mol of acetoaldehyde in an aqueous solution and the urea silicate goes into solution. The unreacted metasilicic acid is filtered out. About 15% to 25% of said metasilicic acid is filtered out. The urea silicate formaldehyde solution is heated to 70° to 110° C. for 20 to 60 minutes, until the desired viscosity is obtained, thereby producing poly (formaldehyde urea silicate) resin. The resin may be produced as a thick clear resin or a solid, depending on the length of time the resin is heated.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04033935
Source datasetuspto-grants-1977_07
ORD IDord-9780204487e14043b91a7386f1fc2080
Source noteuspto-grants-1977_07