HuagongsheHuagongshe Chemistry Print Report · For research reference only
Ethylene → ethylene MMA
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Ethylene | HCID 6325 | — |
| Reactant | Methyl Methacrylate | HCID 6658 | — |
| Solvent | Methanol | HCID 887 | — |
| Product | ethylene MMA | HCID 16212796 | — |
Reaction Steps
2 ml of purified methylmethacrylate (MMA) was charged in the above flask where ethylene polymerization had been conducted, and block copolymerization was initiated at room temperature. After 2 hours, the reaction solution was poured into a large amount of methanol to stop polymerization and to precipitate a polymer. The polymer thus precipitated was filtrated, washed with methanol and dried under reduced pressure to measure its weight. The polymer thus obtained was extracted with chloroform in a Soxhlet apparatus for 4 hours, and the part insoluble in chloroform was taken out and dried to measure its weight. In this manner, 710 mg of white fine powdery ethylene/MMA block copolymer was obtained.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US05527751 |
| Source dataset | uspto-grants-1996_06 |
| ORD ID | ord-48121c46c20b4be8939942a6307576df |
| Source note | uspto-grants-1996_06 |