Isoprene → HCID 86736032, compound
Reaction equation
[CH2:1]=[CH:2][C:3](=[CH2:5])[CH3:4].[CH:6]([Li])([CH2:8][CH3:9])[CH3:7]>C1CCCCC1>[CH2:1]=[CH:2][C:3](=[CH2:4])[CH3:5].[CH2:9]=[CH:8][C:6]1[CH:7]=[CH:4][CH:3]=[CH:2][CH:1]=1.[CH2:1]=[CH:2][C:3](=[CH2:4])[CH3:5]Participants
Reagents, catalysts & solvents 1
Procedure
A living poly(isoprene/styrene/isoprene) three block copolymer was prepared by polymerizing isoprene (151.3 g) in cyclohexane (1362 g) solution. Polymerization was initiated by the addition of 79.5 ml of a 95 mmole/liter solution of secondary butyllithium. The reaction was continued for 2.5 hours at 50° C. The living polyisoprene (number average molecular weight 25,600) solution formed was then reacted with styrene (37.9 g) and the reaction was continued for a further 2.5 hours at 50° C. The living poly(isoprene/styrene) block copolymer (number average molecular weight 31,200) solution formed was then reacted with a further amount of isoprene (151.3 g) and the reaction was continued for a further 2.5 hours at 50° C. The number average molecular weight of the living poly(isoprene/styrene/isoprene) block copolymer was 54,400.
Workup
- customPolymerization
Sources & evidence
- ORD record
- ord-5e2a734b130f4b8c9de65673851dcfe4
- Source dataset
- uspto-grants-1979_05
- Patent number
- US04156673
Reaction notes
Loading…