Sulfuric Acid → p-Hydroxystyrene p-tetrahydropyranyloxystyrene
https://huagongshe.com/reaction/2674
Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Sulfuric Acid | HCID 1118 | — |
| Reactant | 3,4-dihydro-2H-pyran | HCID 8080 | — |
| Reactant | Sodium Carbonate | HCID 10340 | — |
| Reactant | 4-Ethynylphenol | HCID 32758 | — |
| Solvent | Water | HCID 962 | — |
| Solvent | 1,2-Dimethoxyethane | HCID 8071 | — |
| Product | p-Hydroxystyrene p-tetrahydropyranyloxystyrene | HCID 67686066 | — |
Reaction Steps
Poly(p-hydroxystyrene) (weight average molecular weight: 9,600) in an amount of 9 g was dissolved in 100 ml of dimethoxyethane, and thereto 12.6 g of 3,4-dihydro-2H-pyran and 0.5 ml of sulfuric acid were added. This solution was stirred for 15 hours at 30°-40° C. After the reaction was completed, the reaction solution was concentrated under reduced pressure. The residue obtained was neutralized with sodium carbonate, and then poured into water to precipitate crystals. The crystals were filtered off, washed with water and dried under reduced pressure. Thus, 11.0 g of poly(p-tetrahydropyranyloxystyrene-p-hydroxystyrene) was obtained as white powder. The ratio of the p-tetrahydropyranyloxystyrene units to the p-hydroxystyrene units in the polymer obtained was determined to be 3:7 by 1H-NMR analysis.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US05731123 |
|---|
| Source dataset | uspto-grants-1998_03 |
|---|
| ORD ID | ord-5a412429988a4f6d803dc50ce52e1efd |
|---|
| Source note | uspto-grants-1998_03 |
|---|