참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|
| 반응물 | Methanol | HCID 887 | — |
| 반응물 | Toluene | HCID 1140 | — |
| 생성물 | Styrene-butadiene-styrene | HCID 22280236 | — |
반응 단계
In a 100-ml of toluene was dissolved 5 g of the polymer produced above. The resulting solution was subjected to high speed centrifugation at 10,000 rpm to separate it into a toluene-soluble portion (A) and a toluene-insoluble portion (I). The toluene-insoluble portion was 20.2% of the original polymer. Methanol was added in small portions to the toluene-soluble portion to precipitate part of the polymer of the toluene-soluble portion and thus Sample B was obtained. Then, a large amount of methanol was added to the residue to obtain Sample C. Thus, the toluene-soluble portion of the original polymer was subjected to fractional precipitation to obtain Samples B and C. Incidentally, the styrene-butadiene-styrene block copolymer produced in the first step of polymerization was named "Sample S".
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 특허 번호 | US04588782 |
|---|
| 출처 데이터셋 | uspto-grants-1986_05 |
|---|
| ORD ID | ord-1c62778477324394958c98e21bca8dd7 |
|---|
| 출처 메모 | uspto-grants-1986_05 |
|---|