Ethylene → Furan-2,5-dione--ethene (1/1)
Reaction equation
C=C.[C:3]1(=[O:9])[O:8][C:6](=[O:7])[CH:5]=[CH:4]1>>[CH2:3]=[CH2:4].[C:6]1(=[O:7])[O:8][C:3](=[O:9])[CH:4]=[CH:5]1Participants
3
Conditions
- Temperature
- 500 °C
Procedure
An ethylene/maleic anhydride trunk copolymer was prepared which contained 86.5 weight percent ethylene and 13.5 weight percent maleic anhydride. The copolymer was pumped by an extruder through a tube heated to about 500° C. to reduce the molecular weight. The melt viscosity was 600 centipoises at 140° C. The average chain length was about 300 carbon atoms.
Workup
- customThe copolymer was pumped by an extruder through a tube
- customat 140° C
Sources & evidence
- ORD record
- ord-131f3d3a81354c29bda3691d2278ed64
- Source dataset
- uspto-grants-1980_09
- Patent number
- US04225476
Reaction notes
Loading…