Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Pyridine | HCID 1049 | — |
| Reactant | p-Toluenesulfonic acid | HCID 6101 | — |
| Reactant | Ethyl vinyl ether | HCID 8023 | — |
| Reactant | HCID 131722471 | HCID 131722471 | — |
| Solvent | Water | HCID 962 | — |
| Solvent | Dimethylformamide | HCID 6228 | — |
| Product | HCID 131722470 | HCID 131722470 | — |
Reaction Steps
50g of poly(hydroxystyrene/t-butoxycarbonylmethoxystyrene/morpholinylcarbonylmethoxystyrene) where 8.4% of hydroxy groups in polyhydroxystyrene was substituted into t-butoxycarbonylmethoxy group and 5% of hydroxy groups into morpholinylcarbonylmethoxy group, so obtained from Synthesis example 3, was dissolved in 500 ml dimethyl formamide. With the addition of p-toluene sulfonic acid in catalytic amount, the reacting mixture was stirred at 20° C., followed by the addition of ethylvinyl ether (14 g). After reaction for 1 hour, the mixture was neutralized with pyridine, followed by dropwise adding into 5 L water to obtain a white solid. The solid, so formed, was filtered off, washed with distilled water for dehydration and dissolved again in acetone. Then, the reacting solution dropwise added into 5 L water for filtration and washed, for dehydration and drying. Thus, a resin, so obtained, was 52g of poly(hydroxystyrene/ethoxyethoxystyrene/t-butoxycarbonylmethoxystyrene/morpholinocarbonyl lmethoxystyrene) having the weight average molecular weight of 14,400 as polystyrene, in which 16% of hydroxy groups in polyhydroxystyrene was substituted into ethoxyethoxy group, 8.4% of hydroxy groups into t-butoxycarbonylmethoxy group and 5% of hydroxy groups into morpholinylcarbonylmethoxy group.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US06210859B1 |
|---|
| Source dataset | uspto-grants-2001_04 |
|---|
| ORD ID | ord-7011ec05a02c49fd83b1c2f270dacd92 |
|---|
| Source note | uspto-grants-2001_04 |
|---|