反应详情
EQUATION
反应方程式
REACTANTS
反应物
PRODUCTS
生成物
AUXILIARIES
试剂、催化剂与溶剂
CONDITIONS
反应条件
- 温度
- 77.5 °C
PROCEDURE
实验过程
The Dextromethorphan Resin Complex was prepared by first dissolving 954 g of dextromethorphan HBr in 8 liters of purified water heated to 75-80° C., and then slowly adding 1,758 g of AMBERLITE™ IRP-69 resin with continuous mixing while cooling down to room temperature. The dispersion was mixed for 4 hours and upon completion, allowed to settle before decanting the supernatant. The slurring/decanting process was repeated twice with sufficient amounts of purified water. The wet resin complex was then dried in a VWR™ convection oven maintained at 50° C. until moisture content was about 20-25%. In a separate container, KOLLIDON K-30 polymer (116 g) was dissolved in 1,150 g of purified water and slowly applied to the wet resin complex in a Hobart type mixer (Kitchen Aid) to form a uniform mass. The wet mass was then dried at 50° C. in a VWR™ convection oven to the moisture content was around 4-6%. The dried granules were then milled through a 40 mesh screen using CO-MIL™ brand mill.
WORKUP
后处理
- additionslowly adding 1,758 g of AMBERLITE™
- additionresin with continuous mixing
- temperaturewhile cooling down to room temperature
- additionThe dispersion was mixed for 4 hours and upon completion
- custombefore decanting the supernatant
- customThe wet resin complex was then dried in a VWR™ convection oven
- temperaturemaintained at 50° C. until moisture content
- dissolutionIn a separate container, KOLLIDON K-30 polymer (116 g) was dissolved in 1,150 g of purified water
- customto form a uniform mass
- customThe wet mass was then dried at 50° C. in a VWR™ convection oven to the moisture content
- customThe dried granules were then milled through a 40 mesh screen