Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 342341Generated: October 30, 2026

Ammonia → Glycidyl methacrylate

https://huagongshe.com/reaction/342341

Reaction equation

Participants

RoleNameHCIDCharge
ReactantAmmoniaHCID 222—
Reactanttert-Butyl hydroperoxideHCID 6410—
ReactantErythorbic AcidHCID 54675810—
SolventWaterHCID 962—
ProductGlycidyl methacrylateHCID 7837—

Reaction Conditions

Temperature50 °C

Reaction Steps

The initiator solution consisted of 2.5 g of 70% t-butyl hydroperoxide dissolved in 25 g of water and the reducing agent solution consisted of 1.4 g of erythorbic acid, 0.5 g of aqua ammonia, and 25 g of water. The reactor contents were heated to 50° C. and 52.8 g of monomer mixture #1 was added to the reactor. Two ml of the initiator solution and 1 ml of the reducing agent solution were separately added to the reactor. Polymerization was started. The remaining monomer mixture #1 was added over a 60 minute period followed by a 30 minute addition of monomer mixture #2. The remaining initiator and reducing agent solutions were added over a 105 minute period. After completion of the additions, the polymer dispersion was held at 70° C. for 30 minutes. The polymer dispersion was checked by gas chromatographic analysis for residual unreacted monomer. The monomer content was less than 1000 ppm. The dispersion was cooled to room temperature and the physical properties determined.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS05858524
Source datasetuspto-grants-1999_01
ORD IDord-3e0c5a39e6ec487da63c4837634bdb06