(Comparison) 1600 kg of water glass with an SiO2/Na2O ratio of 2.06 and an active substance content of 45.5% were admixed with 36.8 kg of sodium hydroxide solution (48% strength) and spray-dried in a spray tower from Kestner to give an amorphous sodium silicate having an active substance content of 83%. 15 kg of the amorphous sodium silicate are heat-treated at 720° C. for 90 min in a muffle furnace (Nabertherm, model W1000/H). A second batch is treated identically. The chilled materials (about 24 kg) are pulverized using a jaw crusher and a disk mill.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US06743766B1 |
| Source dataset | uspto-grants-2004_06 |
| ORD ID | ord-ee6f125aac904e21a82a287e76f823af |
| Source note | uspto-grants-2004_06 |