Sodium Hydroxide → Sodium orthosilicate
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Sodium Hydroxide | HCID 14798 | — |
| Reactant | Sodium Silicate | HCID 23266 | — |
| Product | Sodium orthosilicate | HCID 26051 | — |
Reaction Steps
50 kg of water glass having an SiO2/Na2O of 3.45 and an active substance content of 36.1 % (grade Na 4/1 from Clariant France S.A.) were admixed with 6.51 kg of sodium hydroxide solution (48% strength) and spray-dried in a laboratory spray dryer (spray tower) from Anhydro to give an amorphous sodium silicate having an active substance content of 83%. 15 kg of the amorphous sodium silicate are heat-treated at 720° C. for 90 min in a muffle furnace (Nabertherm, model W1000/H). The chilled material (about 10 kg) is pulverized using a jaw crusher and a disk mill.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US06743766B1 |
| Source dataset | uspto-grants-2004_06 |
| ORD ID | ord-95079ea276874a3facad32187666f02b |
| Source note | uspto-grants-2004_06 |