Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 371779Generated: October 25, 2026

Formaldehyde → Urea, polymer with formaldehyde and 1,3,5-triazine-2,4,6-triamine

https://huagongshe.com/reaction/371779

Reaction equation

Participants

RoleNameHCIDCharge
ReactantFormaldehydeHCID 712—
ReactantSulfur DioxideHCID 1119—
ReactantUreaHCID 1176—
ReactantMelamineHCID 7955—
SolventWaterHCID 962—
SolventO-XyleneHCID 7237—
ProductUrea, polymer with formaldehyde and 1,3,5-triazine-2,4,6-triamineHCID 168250—

Reaction Conditions

Temperature65 °C

Reaction Steps

A urea-formaldehyde-melamine prepolymer solution is prepared from 165 grams of 37% aqueous formaldehyde, 45 grams of water, 89 grams of urea and 1 gram of melamine, adjusted to pH 9.3 and heated for 1 hour at 65° C. One-hundred seventy grams of this prepolymer solution are emulsified in a solution of six grams of Tetronic 1502 dissolved in one-hundred grams of xylene, and 0.06 milliequivalents of sulfur dioxide (about 4 normal in xylene solution) is added, resulting in an exothermic reaction. After stirring for 1 hour, the solvent dispersion has little or no precipitate. Without any preliminary phase separation, the product is mixed with water to give about 16% total solids, and this "aqueous redispersion" is steam distilled under high-shear agitation to yield a product free of of residual xylene, closely resembling that described in Example 1. A paper coating prepared as described in Example 1 has a scatter coefficient of about 4,000 cm2 /gram.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04087581
Source datasetuspto-grants-1978_05
ORD IDord-112bde496d874acc9ee709703c6c59ac
Source noteuspto-grants-1978_05