Acrylamide → Acrylamide-acrylic acid resin
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Acrylamide | HCID 6579 | — |
| Reactant | Acrylic Acid | HCID 6581 | — |
| Reactant | Sodium Hydroxide | HCID 14798 | — |
| Reactant | Ammonium Persulfate | HCID 62648 | — |
| Solvent | Water | HCID 962 | — |
| Product | Acrylamide-acrylic acid resin | HCID 62693 | — |
Reaction Steps
In a reactor similar to Example 1, a monomer mixture containing 622.0 grams of acrylamide, 54.8 grams of acrylic acid, 168.4 grams of 10% NaOH and 182 grams of water was allowed to react with a catalyst mixture containing 1.3 grams of ammonium persulfate in 198 grams of water at refluxing temperature. Water was used as a solvent in amount of 1934.0 grams
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US04088530 |
| Source dataset | uspto-grants-1978_05 |
| ORD ID | ord-cd09d6336b994885940ef8d9e1c38257 |
| Source note | uspto-grants-1978_05 |