HRID372666
反应详情
EQUATION
反应方程式
REACTANTS
反应物
PRODUCTS
生成物
AUXILIARIES
试剂、催化剂与溶剂
PROCEDURE
实验过程
One operates under the same polymerization conditions in 250 cc. Steinie bottles, in heptane medium (123 g.) with 9.24 g. of isoprene and 3.08 g. of styrene (25% referred to the isoprene). Copolymerization is effected for 2 hours at 70° C. in the presence of 50 × 10-6 moles of active n-BuLi.
WORKUP
后处理
- customOne operates under the same polymerization conditions in 250 cc
- customCopolymerization