Glycolic Acid → Poliglecaprone

https://huagongshe.com/reaction/379495

Reaction equation

Participants

RoleNameHCIDCharge
ReactantGlycolic AcidHCID 757—
Reactant2-ethylhexanoic acid tin(II) saltHCID 9318—
Reactantepsilon-CAPROLACTONEHCID 10401—
ReactantGlycolideHCID 65432—
ProductPoliglecaproneHCID 65431—

Reaction Conditions

Temperature150 °C

Reaction Steps

Glycolide (0.21 moles) was mixed with ε-caprolactone (4.0 moles) and a catalytic amount of stannous octoate (0.8 mole) and glycolic acid (0.40 moles). The system was heated to 150° C. and was stirred at this temperature for 14 hours. At the conclusion of the reaction, the unreacted monomer was removed by heating at 120° C. under reduced pressure for 1 hour. The resulting polymer had a peak melting temperature of 54.3° C. as measured by DSC.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS06299631B1
Source datasetuspto-grants-2001_10
ORD IDord-515a6a6c9ec040f88ec84ca01eb6da11
Source noteuspto-grants-2001_10