In this way, the reaction was conducted for 48 hours while continuously adding the aqueous solution of mixture of nickel nitrate, cobalt nitrate and aluminum nitrate, aqueous ammonia and the aqueous solution of sodium hydroxide to the reactor and continuously taking the resulting reaction mixture (slurry) out of the reactor. After 48 hours from the start of the reaction, the resulting slurry was filtered, washed with water and dried to provide a powder of nickel cobalt aluminum hydroxide.
WORKUP
后处理
- additionwhile continuously adding
- customthe resulting reaction mixture (slurry) out of the reactor
- customAfter 48 hours from the start of the reaction
- filtrationthe resulting slurry was filtered
- washwashed with water
- customdried