Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Isoprene | HCID 6557 | — |
| Reactant | Styrene | HCID 7501 | — |
| Reactant | Cyclohexane | HCID 8078 | — |
| Solvent | Isopropanol | HCID 3776 | — |
| Product | HCID 19842620 | HCID 19842620 | — |
Reaction Steps
A stainless autoclave dried well and flushed with nitrogen was charged with 266 g of styrene and 2,500 g of cyclohexane. After the solution had been heated to 40° C., 3.5 mL of a 1.0 M hexane solution of n-butyllithium was added thereto, it was heated to 50° C. and reacted for 2 hours. 60 g of isoprene was then added as a cyclohexane solution and reacted for a further 2 hours. 266 g of styrene and 700 g of cyclohexane were then added and reacted for a further 2 hours. After the reaction was completed, 0.7 g of isopropanol was added to give a styrene-isoprene-styrene block copolymer. The average molecular weight obtained by GPC was 107,000, and the molecular weight distribution was 1.45.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US06806322B2 |
|---|
| Source dataset | uspto-grants-2004_10 |
|---|
| ORD ID | ord-80eaad69f2b94b82a84f6aac2dcb7c21 |
|---|
| Source note | uspto-grants-2004_10 |
|---|