epsilon-CAPROLACTONE → epsilon-Caprolactone p-Dioxanone
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | epsilon-CAPROLACTONE | HCID 10401 | — |
| Reactant | Dioxanone | HCID 18233 | — |
| Product | epsilon-Caprolactone p-Dioxanone | HCID 86748302 | — |
Reaction Steps
The procedure in Example 5A is substantially repeated except that 45.7 grams (0.40 mole) of ε-caprolactone and 61.3 grams (0.60 mole) of p-dioxanone were used. The copolymer was dried under vacuum (0.1 mm Hg) at 80° C. for about 80 hours to remove any unreacted monomer. The copolymer had an inherent viscosity of 0.18 dL/g in HFIP at 25° C. The copolymer was a liquid at room temperature. The molar ratio of PCL/PDS was found to be 46.7/53.3 by proton NMR.