Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 405653Generated: October 25, 2026

Ethyl Acetate → MAU potassium 3-methacryloxypropanesulfonate

https://huagongshe.com/reaction/405653

Reaction equation

Participants

RoleNameHCIDCharge
ReactantEthyl AcetateHCID 8857—
Reactant11-(Methacryloylamino)undecanoic acidHCID 2764185—
ReactantPotasium 3-sulphopropyl methacrylateHCID 23682747—
CatalystAzobisisobutyronitrileHCID 6547—
SolventMethanolHCID 887—
ProductMAU potassium 3-methacryloxypropanesulfonateHCID 131731612478.2%

Reaction Conditions

Temperature60 °C

Reaction Steps

In 59.69 g of methanol were dissolved 18.15 g (67.41 mmol) of 11-methacrylamidoundecanoic acid (MAU), 1.85 g (7.49 mmol) of potassium 3-methacryloxypropanesulfonate (Tokyo Chemical industry Co.), and 0.31 g (1.89 mmol) of azobisisobutyronitrile (Nacalai Tesque, Inc.). The solution was deaerated by bubbling nitrogen for 60 minutes. The container was covered with a septum, and the polymerization was conducted by heating at 60° C. for 20 hours. After the completion of the polymerization reaction, the reaction solution was dropwise added into a large excess of ethyl acetate, and the resulting precipitate was collected by filtration under suction. After drying under reduced pressure, 18.47 g of random MAU/potassium 3-methacryloxypropanesulfonate copolymer (90/10) was obtained (yield: 92.4%). The weight average molecular weight was 240000.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS08753686B2
Source datasetuspto-grants-2014_06
ORD IDord-afe1d64d88df42dfb71c051d1640df24
Source noteuspto-grants-2014_06