Reaction equation

Participants

RoleNameHCIDCharge
ReactantPhenolphthaleinHCID 4764—
ReactantEpichlorohydrinHCID 7835—
ProductBenzofuransHCID 253613—

Reaction Steps

(A-1) 159 g of 3,3-bis(4-hydroxyphenyl)-2-benzofuran-1-on, 426.6 g of epichlorohydrin, and 160 g of a 50% alkali aqueous solution are mixed in a 1 L flask and then reacted together at 95° C. for 1 hour to form a bisphenylbenzofuran-type epoxy resin. 215 g of the bisphenylbenzofuran-type epoxy resin is mixed with 450 mg of triethylbenzylammoniumchloride, 100 mg of 2,6-diisobutylphenol, and 72 g of acrylic acid. The mixture is heated and completely dissolved at a temperature ranging from 90 to 120° C., while air is blown therein at a speed of 25 Ml per minute.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS08530537B2
Source datasetuspto-grants-2013_09
ORD IDord-80bee22462ef451986276d8676dcb69f