HRID414111
反应详情
EQUATION
反应方程式
REACTANTS
反应物
PRODUCTS
生成物
AUXILIARIES
试剂、催化剂与溶剂
PROCEDURE
实验过程
In order to prepare the test coating, 100 grams of the above oligomer were mixed with 0.1 gram of T-12 tin catalyst, and 20 grams of EEP solvent. A second component was prepared from 126.4 grams of isocyanate multifunctional oligomer biurets formed by the reaction product between hexamethylene diisocyanate and water and 20 g of EEP solvent. Three mil wet films were cast from the mixed components which dried hard in two hours and had a Sward hardness of 10 in 24 hours.