HRID426509

反应详情

EQUATION

反应方程式

HRID 426509 的结构方程式

PROCEDURE

实验过程

The said urea silicate is mixed with an aqueous formaldehyde solution in the ratio of 1:1 mols, heated to 70° to 100° C. while agitating, for 20 to 60 minutes, or until the desired viscosity is reached, thereby producing poly (formaldehyde urea silicate) resin, which is clear in color and may be produced as a thick liquid or as a solid.

WORKUP

后处理

  1. temperature1 mols, heated to 70° to 100° C.