Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 435512Generated: October 25, 2026

Ethylene glycol dimethacrylate → 9-Ethenylcarbazole;oxiran-2-ylmethyl 2-methylprop-2-enoate

https://huagongshe.com/reaction/435512

Reaction equation

Participants

RoleNameHCIDCharge
ReactantEthylene glycol dimethacrylateHCID 7355—
ReactantStyreneHCID 7501—
ReactantPotassium PersulfateHCID 24412—
ReactantTrisodium phosphate dodecahydrateHCID 61473—
ReactantSodium Lauryl SulfateHCID 3423265—
ReactantPavettineHCID 15114296—
SolventWaterHCID 962—
SolventDichloromethaneHCID 6344—
Product9-Ethenylcarbazole;oxiran-2-ylmethyl 2-methylprop-2-enoateHCID 131713079—

Reaction Steps

A 300-mL roundbottomed flask, equipped with a distillation head and a mechanical stirrer, is utilized. 200 mL of water containing 0.5 g of potassium persulfate, 0.5 g of trisodium phosphate dodecahydrate, and 1.5 g of sodium dodecyl sulfate are heated to 70° C. under a nitrogen atmosphere. A seed emulsion is formed by adding 4.5 mL of styrene and 0.5 mL of ethylene glycol dimethacrylate. After 30 min the seed emulsion has a particle size of 0.021 μm and pH of 8.5. A solution of 20 g of vinyl carbazole and one gram of "Aerosol" OT-100 in 10 mL of dichloromethane is then added at a rate of 0.1 mL/min. The dichloromethane is removed by distillation as soon as it is added. After the core emulsion is complete, 0.1 g of potassium persulfate in 10 mL of water is added, and then 2.5 mL of glycidyl methacrylate is added at a feed rate of 0.1 mL/min. 45 min is allowed for the polymerization. The final particle size is 0.041 μm. The final solids content is 10.5%.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04401765
Source datasetuspto-grants-1983_08
ORD IDord-fbc68e328262418582848ce10155d742