HRID439682
反应详情
EQUATION
反应方程式
REACTANTS
反应物
PRODUCTS
生成物
AUXILIARIES
试剂、催化剂与溶剂
PROCEDURE
实验过程
Into a 189 liter (50 gallon) stainless steel reactor, charge 62.6 kg. (137.8 lbs.) of double-bond isomerized-octadecenyl succinic anhydride (Dixie Chemical Company, Inc.) and 13.1 kg. (28.8 lbs.) of 150 solvent neutral (S150N) mineral oil. Heat the contents of the reactor to 130° C.±10° C. under a nitrogen atmosphere and stir at a speed of 150 rpm. Charge 15 kg. (33 lbs.) of tetraethylene pentamine (Union Carbide "Ultra High Purity" grade) below the surface of the reactor contents and heat the contents to 160° C.±5° C. Strip with nitrogen for approximately 21/2 hours or until water no longer evolves.
WORKUP
后处理
- additionInto a 189 liter (50 gallon) stainless steel reactor, charge 62.6 kg
- temperatureHeat the contents of the reactor to 130° C.±10° C. under a nitrogen atmosphere
- additionCharge 15 kg
- custom2 hours