Toluene → 1-Propyl-1,1,3,3-tetramethyldisiloxane
https://huagongshe.com/reaction/452286
Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Toluene | HCID 1140 | — |
| Reactant | Propylene | HCID 8252 | — |
| Reactant | Tetramethyl disiloxane | HCID 57376941 | — |
| Catalyst | Chlorotris(triphenylphosphine)rhodium(I) | HCID 84599 | — |
| Product | 1-Propyl-1,1,3,3-tetramethyldisiloxane | HCID 59985306 | — |
Reaction Steps
An 80 mL Fischer-Porter high pressure bottle was charged with tetramethyldisiloxane (10.0 g), toluene (10.0 g) and Wilkinson's catalyst ((PPh3)3RhCl, 40 ppm), stirred and brought to 50° C. The bottle was attached to a manifold and pressurized with propylene (40 psig) and maintained at 50° C. for 2 h. The pressure was vented, and the reaction was sampled for GC analysis; found M′MR product and MRMR byproduct (40:60). The resulting mixture of materials was used without further purification, yield 14.1 g.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US08491876B2 |
|---|
| Source dataset | uspto-grants-2013_07 |
|---|
| ORD ID | ord-854a1dd0844d46528a4e3cef1877cdb1 |
|---|
| Source note | uspto-grants-2013_07 |
|---|