Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 460399Generated: October 25, 2026

Sulfuric Acid → Acrylonitrile butadiene styrene

https://huagongshe.com/reaction/460399

Reaction equation

Participants

RoleNameHCIDCharge
ReactantSulfuric AcidHCID 1118—
ReactantStyreneHCID 7501—
Reactant1,3-ButadieneHCID 7845—
ReactantAcrylonitrileHCID 7855—
ReactantTetrasodium PyrophosphateHCID 24403—
Reactant(2R,3S,4R,5R)-2,3,4,5,6-pentahydroxyhexanalHCID 107526—
ReactantPotassium OleateHCID 23665571—
SolventWaterHCID 962—
ProductAcrylonitrile butadiene styreneHCID 24756—

Reaction Steps

50 parts of butadiene rubber latex powder, 36 parts of styrene, 14 parts of acrylonitrile, and 150 parts of deionized water were blended. To the blend, 1.0 parts of potassium oleate, 0.4 parts of cumenhydroperoxide, 0.2 parts of mercaptan-containing chain transfer agent, 0.4 parts of glucose, 0.01 parts of ferrous sulfate hydrate, and 0.3 parts of sodium pyrophosphate were added. The blend was kept at 75° C. for 5 hours to obtain g-ABS latex. To the g-ABS latex, 0.4 parts of sulfuric acid was added, coagulated and dried to obtain acrylonitrile-butadiene-styrene graft copolymer resin (g-ABS) in a powder form.