Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 462480Generated: October 25, 2026

Acrylamide → Acrylamide-acrylic acid resin

https://huagongshe.com/reaction/462480

Reaction equation

Participants

RoleNameHCIDCharge
ReactantAcrylamideHCID 6579—
ReactantAcrylic AcidHCID 6581—
SolventWaterHCID 962—
ProductAcrylamide-acrylic acid resinHCID 62693—

Reaction Conditions

Temperature30 °C

Reaction Steps

56 grams 50% acrylamide, 12 grams acrylic acid and 127 grams water were mixed, and warmed up to 30° C. Nitrogen was used to purge the flask. Then 0.7 gram ammonium persulfate in 3 grams of water and 0.7 gram sodium metabisulfite in 3 grams water were added, respectively. After 20 minutes, the reaction began to take place, the temperature slowly rose to 78° C. (max.) after stirring for 1.5 hour a 20% copolymer was thus produced with an acrylamide/acrylic acid ratio of 70/30. 7 grams NaOH in 30 grams water was then added to neutralize the copolymer.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04515855
Source datasetuspto-grants-1985_05
ORD IDord-afb2cfbf8f8b4735958f3371f9372578
Source noteuspto-grants-1985_05