Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Acrylic Acid | HCID 6581 | — |
| Reactant | Isobutyl Methacrylate | HCID 7352 | — |
| Reactant | Butyl Methacrylate | HCID 7354 | — |
| Reactant | Butyl Acrylate | HCID 8846 | — |
| Reactant | tert-Butyl peroxybenzoate | HCID 11966 | — |
| Solvent | Isopropanol | HCID 3776 | — |
| Solvent | 2-Butoxyethanol | HCID 8133 | — |
| Product | Isobornylmethacrylate | HCID 71311141 | — |
Reaction Steps
One hundred twenty-five parts of butyl Cellosolve is heated to 150° C. and a monomer mix consisting of 200 parts of isobutyl methacrylate, 137.5 parts of n-butyl methacrylate, 50 parts of n-butyl acrylate, 62.5 parts of acrylic acid and 50 parts of methacryloxyethyl esters of linseed oil fatty acids and an initiator solution consisting of 1.5 parts of t-butyl perbenzoate dissolved in 10 parts of butyl Cellosolve are added to the 150° C. solvent over three hours at a constant rate. Reaction temperature is held at 150±2° C. throughout the gradual additions and for 15 minutes after the addition of an initiator chaser solution consisting of 3 parts of t-butyl perbenzoate dissolved in 10 parts of butyl Cellosolve. The polymer solution is then cooled to 100° C. and diluted with 174 parts of isopropanol.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US04547556 |
|---|
| Source dataset | uspto-grants-1985_10 |
|---|
| ORD ID | ord-41730fe9ee214c4fb80466baa1fae14c |
|---|
| Source note | uspto-grants-1985_10 |
|---|