HuagongsheHuagongshe Chemistry Print Report · For research reference only
Water → Sodium orthosilicate
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Water | HCID 962 | — |
| Reactant | Sodium Silicate | HCID 23266 | — |
| Product | Sodium orthosilicate | HCID 26051 | — |
Reaction Steps
A reaction mixture having the molar composition 0.303 Na2O:0.0052 Al2O3 :SiO2 :30 H2O is first prepared by adding 83.5 parts by weight of soda waterglass (27% of SiO2, 8.43% of Na2O and 0.24% of Al2O3) to 149 parts of water. Some of a filter-moist crystalline sodium silicate from a previous experiment (71% weight loss as a result of heating to 1200° C.; only the amount of water was taken into account in calculating the molar composition) is then added. 4.93 parts of 96% strength sulfuric acid are then added slowly, while stirring. The reaction mixture then has the following molar composition: 0.174 Na2O:0.0052 Al2O3 :SiO2 :0.129 Na2SO4 :30 H2O.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US04578258 |
| Source dataset | uspto-grants-1986_03 |
| ORD ID | ord-b829addfec144865ad277f626ea6a16c |
| Source note | uspto-grants-1986_03 |