HRID484354
反应详情
EQUATION
反应方程式
REACTANTS
反应物
PRODUCTS
生成物
PROCEDURE
实验过程
A butadiene/2-methoxyethyl acrylate copolymer was synthesized as per Example 6, starting with 40 parts of butadiene and 60 parts of 2-methyoxyethyl acrylate. The isolated rubber exhibited a glass transition temperature of -60° C. and a Mooney viscosity of 37 (ML[4,100° C.]).