HuagongsheHuagongshe Chemistry Print Report · For research reference only
Formaldehyde → Benzene, ethenyl-, polymer with 1,3-butadiene
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Formaldehyde | HCID 712 | — |
| Reactant | Acetic Anhydride | HCID 7918 | — |
| Reactant | 2-Naphthalenesulfonic acid | HCID 8420 | — |
| Reactant | Potassium Hydroxide | HCID 14797 | — |
| Reactant | Sodium | HCID 5360545 | — |
| Solvent | Water | HCID 962 | — |
| Product | Benzene, ethenyl-, polymer with 1,3-butadiene | HCID 62697 | — |
Reaction Steps
14.7 kg of Latex A-1 and 2.5 kg of deionized water are charged into a 40 l reactor equipped with a stirrer, heating and cooling apparatus, and a raw material supplying tube. Then, 72 g of acetic anhydride and 1.4 kg of deionized water are added and mixed at 40° C. After stirring and mixing for about 1 minute, the mixture is allowed to stand for 10 minutes. Then, 30 g of the sodium salt of a condensate of beta-naphthalene sulfonic acid and formaldehyde; 110 g of potassium hydroxide (48%) and 880 g of deionized water are added, while stirring. A butadiene/styrene copolymer rubber latex with an average particle size of 0.25 μm is obtained. The pH of this latex is 7.5 and the solid content is 29.1%.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US05290867 |
| Source dataset | uspto-grants-1994_03 |
| ORD ID | ord-42859893ebe9412da45b86aa42948973 |
| Source note | uspto-grants-1994_03 |