Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Isoprene | HCID 6557 | — |
| Reactant | Styrene | HCID 7501 | — |
| Reactant | 2-Methylbuta-1,3-diene;styrene | HCID 159989 | — |
| Reactant | CID 53628100 | HCID 178418400 | — |
| Solvent | Cyclohexane | HCID 8078 | — |
| Product | HCID 19842620 | HCID 19842620 | — |
Reaction Steps
To a 2.6 liter reactor were charged 1499 g of cyclohexane and 85.8 g of styrene monomer. The mixture was heated to 60° C. and 7.8 ml of a 0.70 molar solution of sec-butyllithium initiator in cyclohexane was added. After 41 minutes, the reaction temperature was reduced to 58° C. and 118.5 grams of isoprene was added. After 39 minutes the living styrene-isoprene diblock polymer was coupled to form a linear styrene-isoprene-styrene triblock polymer by adding 32 ml of 0.12M 1,2-dibromoethane in cyclohexane over a period of 11 minutes. A hindered phenol antioxidant was added to the polymer solution which was then devolatized in a vacuum oven under nitrogen at 100° C. for 3 hours.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US05292819 |
|---|
| Source dataset | uspto-grants-1994_03 |
|---|
| ORD ID | ord-05d0f7a191854de7ab42eac6ba6546dd |
|---|
| Source note | uspto-grants-1994_03 |
|---|