HuagongsheHuagongshe Chemistry Print Report · For research reference only
Hydroquinone → Urethane acrylate
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Hydroquinone | HCID 785 | — |
| Reactant | 2-Hydroxyethyl acrylate | HCID 13165 | — |
| Reactant | Isophorone diisocyanate | HCID 169132 | — |
| Product | Urethane acrylate | HCID 21863578 | — |
Reaction Steps
192.4 g of 1,6-hexanediol and 166.6 g of adipic acid were placed in a reaction vessel and reacted for 6 hours at 220° C. while dehydrating and condensing to obtain 318 g of polyester. 222 g (1 mole) of isophorone diisocyanate were added thereto and reacted for 2 hours at 80° C. Moreover, 116 g (1 mole) of 2-hydroxyethyl acrylate and 1.4 g of hydroquinone were further added thereto and reacted for 3 hours at 80° C. while blowing in air to obtain a urethane acrylate (C-1) having acryloyl groups on both ends of a molecule thereof.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US07776937B2 |
| Source dataset | uspto-grants-2010_08 |
| ORD ID | ord-447af580655f40dd946320e5d877559a |
| Source note | uspto-grants-2010_08 |