関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | Acrylic Acid | HCID 6581 | — |
| 反応物 | Methyl Acrylate | HCID 7294 | — |
| 反応物 | Di-tert-butyl peroxide | HCID 8033 | — |
| 反応物 | Beta-Pinene | HCID 14896 | — |
| 反応物 | Di-tert-amyl peroxide | HCID 25320 | — |
| 反応物 | 2-Propenoic acid, 3-hydroxypropyl ester | HCID 33101 | — |
| 溶媒 | Butyl Acetate | HCID 31272 | — |
| 生成物 | beta-Pinene Methyl Acrylate Hydroxypropyl Acrylate | HCID 68459481 | — |
反応手順
A mixture of 38.7% beta-pinene, 25.0% methyl acrylate, 30.7% hydroxypropyl acrylate, 0.8% acrylic acid and 4.8% di-t-butyl peroxide was continuously fed to a 5 gallon continuous stirred tank reactor at a rate calculated to give a average residence time of 20 minutes. The reactor was maintained at a pressure of 500 psig and a temperature of 365° F. The reaction product was continuously pumped to a 30 gallon flash tank maintained at 20% fill level together with di-t-amyl peroxide (4% by weight on reaction product). The contents of the flash tank were maintained at 300° F. The output from the flash tank was mixed with sufficient butyl acetate in a static mixer to reduce the solids content to 81% and drained into storage containers. The reaction was run for a period of 6.5 hours. The resulting resin had a weight average molecular weight of 5000.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 特許番号 | US07776959B2 |
|---|
| 出典データセット | uspto-grants-2010_08 |
|---|
| ORD ID | ord-ddfe49187fa24d669fa3399f0e0a7bdf |
|---|
| 出典メモ | uspto-grants-2010_08 |
|---|