Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 513971Generated: October 26, 2026

Isoprene → Isoprene butadiene

https://huagongshe.com/reaction/513971

Reaction equation

Participants

RoleNameHCIDCharge
ReactantIsopreneHCID 6557—
ReactantStyreneHCID 7501—
Reactant1,3-ButadieneHCID 7845—
SolventMethanolHCID 887—
ProductIsoprene butadieneHCID 168288—

Reaction Conditions

Temperature50 °C

Reaction Steps

Into a dried pressure vessel purged with nitrogen, 80 L of cyclohexane solvent and 0.34 L of sec-butyllithium initiator (10% by mass solution in cyclohexane) were charged. After raising the temperature to 50° C., 4.0 L of styrene was added to allow the polymerization to proceed for 3 h. Then, the polymerization was allowed to proceed for 4 h after adding a mixed liquid of 14.2 L of isoprene and 11.6 L of butadiene and further for 3 h after adding 4.0 L of styrene. The resultant reaction liquid was poured into 80 L of methanol, and the precipitated solid matter was separated by filtration and dried at 50° C. for 20 h, to obtain a polystyrene block-poly(isoprene/butadiene) block-polystyrene block, triblock copolymer.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS09102849B2
Source datasetuspto-grants-2015_08
ORD IDord-535c8e99255c4eebafa4032744d1ef33
Source noteuspto-grants-2015_08