HuagongsheHuagongshe Chemistry Print Report · For research reference only
Methyl p-toluenesulfonate → Urethane acrylate
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Methyl p-toluenesulfonate | HCID 6645 | — |
| Reactant | Benzoyl chloride | HCID 7412 | — |
| Reactant | Hexamethylene diisocyanate | HCID 13192 | — |
| Product | Urethane acrylate | HCID 21863578 | — |
Reaction Steps
1300 g of HDI (hexamethylene diisocyanate), 1.3 g of benzoyl chloride and 1.3 g of methyl para-toluenesulfonate are initially charged in a 41 four-neck flask while stirring. Within 3 hours, 1456 g of a difunctional polypropylene glycol polyether having a number-average molecular weight of 2000 g/mol are added at 80° C., and the mixture is stirred at the same temperature for a further 1 hour. Subsequently, the excess HDI was distilled off by thin-film distillation at 130° C. and 0.1 torr. The resulting prepolymer has an NCO content of 3.23% and a viscosity of 1650 mPas (25° C.).
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US08852829B2 |
| Source dataset | uspto-grants-2014_10 |
| ORD ID | ord-ef763fcd9b3640449450bd06b778138b |
| Source note | uspto-grants-2014_10 |