Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Calcium Carbonate | HCID 10112 | — |
| Reactant | Phenylphosphonic Acid | HCID 15295 | — |
| Solvent | Water | HCID 962 | — |
| Product | Calcium Carbonate | HCID 10112 | — |
| Product | Calcium phenylphosphonate | HCID 20231666 | — |
Reaction Steps
An aqueous slurry of calcium carbonate was prepared by charging a 300 mL reaction flask equipped with a stirrer with 10.0 g (100 mmol) of calcium carbonate (Escalon #2300 (average particle size, 1.7 μm), available from Sankyo Seifun KK) and 90.0 g of water. An aqueous solution of 11.1 g (70 mmol) of phenylphosphonic acid (Nissan Chemical Industries, Ltd.) dissolved in 62.7 g of water was gradually added dropwise at room temperature (about 25° C.) to this slurry with stirring, thereby effecting a reaction for one hour. The slurry was then filtered and the wet cake was thoroughly rinsed with water. The wet cake was subsequently dried at 200° C. for at least 12 hours, yielding a white powder of calcium phenylphosphonate-containing calcium carbonate.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US09035100B2 |
|---|
| Source dataset | uspto-grants-2015_05 |
|---|
| ORD ID | ord-97b253f541a9404cad12455cc7dea7f2 |
|---|
| Source note | uspto-grants-2015_05 |
|---|