Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Aluminum Stearate | HCID 12496 | — |
| Reactant | Sodium Stearate | HCID 2724691 | — |
| Catalyst | Aluminum Stearate | HCID 12496 | — |
| Catalyst | Lead stearate | HCID 61258 | — |
| Product | Ethylene brassylate | HCID 61014 | 95.9% |
Reaction Steps
To demonstrate the improved yields and increased reaction rates obtained utilizing the mixed metal catalysts of this invention, batch polymerizations were identically conducted using (a) a mixed metal catalyst comprised of aluminum stearate and sodium stearate (1.1 molar ratio), (b) aluminum stearate catalyst, and (c) lead stearate catalyst. These reactions were conducted in accordance with the procedure employed in Example II utilizing 74 grams poly(ethylene brassylate) and 0.5 mole percent of the catalyst. Reactions were carried out at 310°-320° C. and 0.1-0.5 mm Hg for four hours. The amount of distillate (crude ethylene brassylate) recovered was recorded after the first hour of reaction. With the mixed metal catalyst, 45 mls ethylene brassylate was obtained after one hour and the overall yield was 95.9 percent. With the aluminum stearate, 36 mls crude ethylene brassylate was obtained in the first hour and the overall yield was only 78 percent. Using lead stearate only 25 mls distillate was obtained after one hour and the yield of crude ethylene brassylate was 69.1 percent.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US04499288 |
|---|
| Source dataset | uspto-grants-1985_02 |
|---|
| ORD ID | ord-f34decf4e22947709dc0e5c3cdbeb5b7 |
|---|
| Source note | uspto-grants-1985_02 |
|---|