Styrene → Prop-2-enenitrile--ethenylbenzene (1/1)
Reaction equation
[C:1](#[N:4])[CH:2]=[CH2:3].[CH2:5]=[CH:6][C:7]1[CH:12]=[CH:11][CH:10]=[CH:9][CH:8]=1>>[C:1](#[N:4])[CH:2]=[CH2:3].[CH2:5]=[CH:6][C:7]1[CH:12]=[CH:11][CH:10]=[CH:9][CH:8]=1Participants
3
Procedure
In the same manner as in the preparation of the graft copolymer B-1 but using 50 parts of polybutadiene, 15 parts of acrylonitrile and 35 parts of styrene, emulsion polymerization was carried out to obtain an ABS graft copolymer latex (degree of grafting: 55%, intrinsic viscosity of free acrylonitrile/styrene copolymer: 0.58 dl/g).
Workup
- customIn the same manner as in the preparation of the graft copolymer B-1
Sources & evidence
- ORD record
- ord-eac2ca6fcbea46ce98f817a2ca8cd900
- Source dataset
- uspto-grants-1989_04
- Patent number
- US04824905
Reaction notes