Next, the 1,6-diaminohexane vapor in the condensing chamber 2 was adiabatically expanded, and the introduced modified particles (26) were exposed thereto for 2 minutes. Consequently, a further polymerization reaction between 1,4-butanedisulfonyl chloride and 1,6-diaminohexane took place on the surface of the modified particles (26), forming a film of 1,4-butanedisulfonylchloride-1,6-diaminohexane co-polymer.