Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Acetate | HCID 175 | — |
| Reactant | Toluene | HCID 1140 | — |
| Reactant | Dichloromethane | HCID 6344 | — |
| Reactant | Methyl Ethyl Ketone | HCID 6569 | — |
| Reactant | Silver | HCID 23954 | — |
| Reactant | HCID 178435161 | HCID 178435161 | — |
| Catalyst | Zinc Stearate | HCID 11178 | — |
| Product | Silver behenate | HCID 164971 | — |
Reaction Steps
A uniform dispersion was prepared by dispersing 3 g of zinc stearate, 15 g of triacetyl cellulose, and 500 ml of methylene chloride in a ball mill for 10 hours. One surface of a polyethylene terephthalate film was subjected to a corona discharging treatment, and the above-described dispersion was coated on the treated surface to form a backing layer of 0.5 μm in thickness. Then, on the opposite surface thereof was coated a coating liquid of 10 g of nitrocellulose dissolved in 300 ml of acetate and dried to form an interlayer of 0.3 μm in thickness. 3 g of silver benehate was added to 20 g of a mixture of toluene and methyl ethyl ketone (1/2 by volume ratio), and the mixture was dispersed for about 20 hours in a ball mill to provide a uniform silver behenate suspension. Then, a silver behenate emulsion was prepared by adding the following composition (I) to 1.5 g of the silver behenate suspension.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US04740439 |
|---|
| Source dataset | uspto-grants-1988_04 |
|---|
| ORD ID | ord-ecd9143188074d2db09a93301cdc5787 |
|---|
| Source note | uspto-grants-1988_04 |
|---|