HuagongsheHuagongshe Chemistry Print Report · For research reference only
Triphenylphosphine → HCID 178444282, compound
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Triphenylphosphine | HCID 11776 | — |
| Reactant | HCID 178444252 | HCID 178444252 | — |
| Solvent | O-Xylene | HCID 7237 | — |
| Product | HCID 178444282 | HCID 178444282 | 80% |
Reaction Conditions
| Temperature | 160 °C |
|---|
Reaction Steps
A mixture of 2.63 g of 4-(bromomethyl)-4'-(trans-4-pentylcyclohexyl)biphenyl and 2.2 g of triphenylphosphine in 150 ml of o-xylene was heated to reflux (bath temperature 160° C.) for 15 hours in a sulphonation flask under argon gasification. After cooling, the white precipitate formed was filtered off, washed several times with benzene and dried in a high vacuum (0.1 mmHg) at 80° C. for 1 hour. There were obtained 3.48 g (80%) of [[4'-(trans-4-pentylcyclohexyl)-4-biphenylyl]methyl]triphenylphosphonium bromide as a white powder (m.p. 263°-265° C.) which was used in the following Wittig reaction without additional purification.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US04613208 |
| Source dataset | uspto-grants-1986_09 |
| ORD ID | ord-4459b77d1b48449a94e80b1e81463898 |
| Source note | uspto-grants-1986_09 |