Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 654242Generated: October 31, 2026

Ethylene Oxide → HCID 131717461, compound

https://huagongshe.com/reaction/654242

Reaction equation

Participants

RoleNameHCIDCharge
ReactantEthylene OxideHCID 6354—
ReactantSodium HydroxideHCID 14798—
ReactantSodium AzideHCID 33557—
Reactant2-(Chloromethyl)oxirane--oxirane (1/1)HCID 168228—
ReactantHCID 513618HCID 513618—
SolventDimethylacetamideHCID 31374—
ProductHCID 131717461HCID 131717461—

Reaction Steps

Elastomeric GEC is prepared according to the same previous procedure as in Example 1, except that commercial rubbery Epichlorohydrin-Ethylene Oxide Copolymer (PEEC) is used instead of PECH as the starting material. The copolymer contains about 70% PECH and 30% Ethylene Oxide. For this reason, a weight ratio NaN3 :PEEC of 0.55 is used in this case. Specifically, the reaction for 16 h at 100° C. of 10 g PEEC (MW~9×105) in 50 g DMA and 5 g EG with 5.5 g NaN3 and 1.5 g NaOH will yield 9.0 g (90%) of GEC azido product. This copolymer containing about 70% GAP and 30% Ethylene Oxide has a MW of about 10,000, a Tg of about -55° C. and a functionality (f) of about 3.5.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS05130381
Source datasetuspto-grants-1992_07
ORD IDord-f46c10a2bacf4e34a66b50485e79558e
Source noteuspto-grants-1992_07