Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Toluene | HCID 1140 | — |
| Reactant | Titanium Tetrachloride | HCID 24193 | — |
| Product | HCID 86742816 | HCID 86742816 | — |
Reaction Steps
To the above described solid component were added 40 ml of toluene and titanium tetrachloride so as to give a titanium chloride/toluene volume ratio of 3/2, the temperature being then raised to 80° C. While stirring, a mixed solution of 2 ml of di-n-butyl phthalate and 5 ml of toluene was dropwise added thereto and stirred at 80° C. for 2 hours. The resulting solid material was separated by filtration and washed with 100 ml of toluene 2 times at 75° C. Furthermore, titanium tetrachloride was added thereto so as to give a titanium tetrachloride/toluene volume ratio of 3/2 and stirred at 80° C. for 2 hours. The resulting solid material was separated by filtration at 80° C. and then washed with 100 ml of n-hexane at room temperature 7 times, thus obtaining 3.4 g of a catalyst component.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US05132261 |
|---|
| Source dataset | uspto-grants-1992_07 |
|---|
| ORD ID | ord-4e007b30848e40188492ea2a17d1b1d3 |
|---|
| Source note | uspto-grants-1992_07 |
|---|