Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 734952Generated: October 26, 2026

Ethylene → Ethylene styrene

https://huagongshe.com/reaction/734952

Reaction equation

Participants

RoleNameHCIDCharge
ReactantEthyleneHCID 6325—
ReactantStyreneHCID 7501—
ReactantChloric acid ethanolHCID 21282719—
SolventTolueneHCID 1140—
ProductEthylene styreneHCID 22558332—

Reaction Steps

To a polymerization reactor under high purity nitrogen atmosphere, 10 ml of purified styrene and 20 ml of toluene were introduced and reaction temperature was controlled to 50° C. Ethylene of 4 atm was added to saturate and then 5 ml of methylaluminoxane (2.1 M toluene solution, Akzo Company product) were introduced. 0.44 ml (3.75 mmol of Ti) of toluene solution in which one of the metallocene catalysts is dissolved was added while vigorously agitating. After agitating the reaction mixture for 1 hour, 10 wt % of chloric acid-ethanol solution was added to terminate a reaction, the reactant was filtered, washed with ethanol and dried in a vacuum oven of 50° C. to obtain a final styrene/ethylene copolymer. Polymerization results and physical properties of polymers for each catalyst are shown in Table 3.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS07592401B2
Source datasetuspto-grants-2009_09
ORD IDord-529efbd917ea4573a84b94ac398edaf2
Source noteuspto-grants-2009_09