Styrene → p-Tert-butoxystyrene styrene

HRID 743925Notes

Reaction equation

HRID 743925 reaction equation
[C:1]([O:5][C:6]1[CH:13]=[CH:12][C:9]([CH:10]=[CH2:11])=[CH:8][CH:7]=1)([CH3:4])([CH3:3])[CH3:2].[CH2:14]=[CH:15][C:16]1[CH:21]=[CH:20][CH:19]=[CH:18][CH:17]=1>>[C:1]([O:5][C:6]1[CH:7]=[CH:8][C:9]([CH:10]=[CH2:11])=[CH:12][CH:13]=1)([CH3:4])([CH3:2])[CH3:3].[CH2:14]=[CH:15][C:16]1[CH:21]=[CH:20][CH:19]=[CH:18][CH:17]=1

Participants

3

Procedure

Using p-tert-butoxystyrene (81.1 g, 0.46 mole) and styrene (4.6 g, 0.04 mole), the polymerization and the treatment were carried out in the same manner as described in Synthesis Example 1, (1), to give 77.1 g of poly(p-tert-butoxystyrene/styrene) as white powders having Mw 20000 (GPC with polystyrene calibration). The polymer was found to have p-tertbutoxystyrene unit and styrene unit in a molar ratio of ca. 92:8 based on 1HNMR.

Workup

  1. customthe polymerization
  2. customas described in Synthesis Example 1, (1),

Sources & evidence

ORD record
ord-bbfc2d21028740c7960e10fcf114e870
Source dataset
uspto-grants-1996_09
Patent number
US05558971

Reaction notes

Loading…