4-Methoxystyrene → HCID 86749844, compound
Reaction equation
[C:1]([O:5][C:6]1[CH:13]=[CH:12][C:9]([CH:10]=[CH2:11])=[CH:8][CH:7]=1)([CH3:4])([CH3:3])[CH3:2].[CH3:14][O:15][C:16]1[CH:23]=[CH:22][C:19]([CH:20]=[CH2:21])=[CH:18][CH:17]=1>>[C:1]([O:5][C:6]1[CH:7]=[CH:8][C:9]([CH:10]=[CH2:11])=[CH:12][CH:13]=1)([CH3:4])([CH3:2])[CH3:3].[CH3:14][O:15][C:16]1[CH:23]=[CH:22][C:19]([CH:20]=[CH2:21])=[CH:18][CH:17]=1Participants
3
Procedure
Using p-tert-butoxystyrene (77.6 g, 0.44 mole) and p-methoxystyrene (8.1 g, 0.06 mole), the polymerization and treatment were carried out in the same manner as described in Synthesis Example 1, (1), to give 77.1 g poly(p-tert-butoxystyrene/p-methoxystyrene) as white powder having Mw 20000 (GPC with polystyrene calibration). The polymer was found to have p-tert-butoxystyrene unit and p-methoxystyrene unit in a molar ratio of ca. 88:12 based on 1HNMR.
Workup
- customthe polymerization and treatment
- customas described in Synthesis Example 1, (1),
Sources & evidence
- ORD record
- ord-98d2d04da09844f981294385e6be763c
- Source dataset
- uspto-grants-1996_09
- Patent number
- US05558971
Reaction notes
Loading…