4-Vinylphenol → HCID 68598481, compound

https://huagongshe.com/reaction/743932

Reaction equation

Participants

RoleNameHCIDCharge
Reactant4-VinylphenolHCID 62453—
Reactant1,1-Dimethylethyl 4-ethenylphenyl carbonateHCID 93485—
ProductHCID 68598481HCID 68598481—

Reaction Steps

To a solution of poly (p-tert-butoxycarbonyloxystyrene) (7.0 g) obtained in above (1) in 1,4-dioxane, conc. hydrochloric acid (5 ml) was added and continued to stir under reflux for 2 hours. After cooling, the reaction mixture was poured into H2O (1 l) and the polymer was precipitated. The polymer was filtered by suction, washed with H2O and dried under reduced pressure to give 4.8 g of poly(p-tert-butoxycarbonyloxystyrene/p-hydroxystyrene) as white powder having Mw 10000 (GPC with polystyrene calibration). The polymer was found to have p-tertbutoxycarbonyloxystyrene unit and p-hydroxystyrene unit in a molar ratio of ca. 4:6 based on 1HNMR.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS05558971
Source datasetuspto-grants-1996_09
ORD IDord-1cbd0e872a3c4a368cd471ba9a8e3e8c
Source noteuspto-grants-1996_09